Potrebujeme váš súhlas na využitie jednotlivých dát, aby sa vám okrem iného mohli ukazovať informácie týkajúce sa vašich záujmov. Súhlas udelíte kliknutím na tlačidlo „OK“.
Standard Practice for Evaluating and Qualifying Oilfield and Refinery Corrosion Inhibitors Using Jet Impingement Apparatus
Automaticky preložený názov:
Štandardná prax pre hodnotenie a kvalifikačné ropné polia a rafinérie inhibítory korózie Použitie Jet impingement Prístroje
NORMA vydaná dňa 1.5.2012
Označenie normy: ASTM G208-12
Poznámka: NEPLATNÁ
Dátum vydania normy: 1.5.2012
Kód tovaru: NS-57603
Počet strán: 14
Približná hmotnosť: 42 g (0.09 libier)
Krajina: Americká technická norma
Kategória: Technické normy ASTM
Keywords:
corrosion inhibitor, electrochemical, high-pressure, high-temperature, jet impingement, JI, laboratory evaluation, mass loss, oil-field inhibitors, refinery inhibitors, ICS Number Code 75.100 (Lubricants, industrial oils and related products)
Significance and Use | ||||||||||||||||||||||||||||||||||
5.1 Selection of corrosion inhibitor for oilfield and refinery applications involves qualification of corrosion inhibitors in the laboratory (see Guide G170). Field conditions should be simulated in the laboratory in a fast and cost-effective manner. 5.2 Oilfield and refinery corrosion inhibitors should provide protection over a range of flow conditions from stagnant to that found during typical production conditions. The inhibitors are not equally effective over all flow conditions, so it is important to determine the flow conditions in which they are effective. 5.3 Severity of hydrodynamic conditions depends on the type of laboratory methodology. Typically, rotating cylinder electrode is effective up to 20 Pa of wall shear stress, rotating cage (RC) is effective between 20 and 200 Pa of wall shear stress, and jet impingement (JI) is effective at wall shear stress above 200 Pa (1)3 of wall shear stress. 5.4 The JI test system is relatively inexpensive and uses simple flat specimens. 5.5 In this practice, a general procedure is presented to obtain reproducible results using JI simulating the effects of different types of coupon materials; inhibitor concentrations; oil, gas, and brine compositions; temperature; pressure; and flow. Erosive effects predominate when the flow rate is very high (typically above 500 Pa) or when sand or solid particles are present; however, this practice does not cover the erosive effects. |
||||||||||||||||||||||||||||||||||
1. Scope | ||||||||||||||||||||||||||||||||||
1.1 This practice covers a generally accepted procedure to use the jet impingement (JI) apparatus for evaluating corrosion inhibitors for oilfield and refinery applications in defined flow conditions. 1.2 The values stated in SI units are to be regarded as standard. No other units of measurement are included in this standard. 1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. |
||||||||||||||||||||||||||||||||||
2. Referenced Documents | ||||||||||||||||||||||||||||||||||
|
Historická
1.5.2013
Historická
1.10.2013
Historická
1.11.2012
Historická
1.5.2010
Historická
1.5.2013
Historická
1.10.2009
Posledná aktualizácia: 2024-12-23 (Počet položiek: 2 217 157)
© Copyright 2024 NORMSERVIS s.r.o.