Potrebujeme váš súhlas na využitie jednotlivých dát, aby sa vám okrem iného mohli ukazovať informácie týkajúce sa vašich záujmov. Súhlas udelíte kliknutím na tlačidlo „OK“.
Standard Test Method for Stereological Evaluation of Porous Coatings on Medical Implants (Withdrawn 2024)
Automaticky preložený názov:
Štandardná skúšobná metóda pre stereologických Vyhodnotenie poréznych povlakov na lekárske implantáty
NORMA vydaná dňa 15.3.2015
Označenie normy: ASTM F1854-15
Poznámka: NEPLATNÁ
Dátum vydania normy: 15.3.2015
Kód tovaru: NS-588545
Počet strán: 10
Približná hmotnosť: 30 g (0.07 libier)
Krajina: Americká technická norma
Kategória: Technické normy ASTM
Keywords:
coating gradiants, metallography, porosity, porous coatings, stereology, thickness,, ICS Number Code 11.040.40 (Implants for surgery, prothetics and orthotics)
Significance and Use | ||||
5.1 All these test methods are recommended for elementary quantification of the morphological properties of porous coatings bonded to solid substrates. 5.2 These test methods may be useful for comparative evaluations of different coatings or different lots of the same coating. 5.3 All the methods should be performed on the same set of images of fields. 5.4 A statistical estimate can be made of the distributions of the mean coating thickness and the volume percent void. No estimate can be made of the distribution of intercept lengths. 5.5 There are limits to the accurate characterization of porosity, depending on spacing between the lines in the line grid (or points in the point grid) and the individual and cumulative fields used for the measurements. Increasing the size of the fields, increasing the number of fields, or decreasing the grid spacing will increase the accuracy of the measurements obtained. 5.6 This method may be suitable for ceramic coatings if an accurate coating cross section can be produced. Producing an accurate ceramic coating cross section may require other techniques than standard metallographic techniques. 5.7 For coatings having a mean thickness less than 300 microns, it is not recommended to attempt to determine the volume percent void or the mean intercept length. |
||||
1. Scope | ||||
1.1 This test method covers stereological test methods for characterizing the coating thickness, void content, and mean intercept length of various porous coatings adhering to nonporous substrates. 1.2 A method to measure void content and intercept length at distinct levels (“Tissue Interface Gradients”) through the porous coating thickness is outlined in 9.4. 1.3 The values stated in SI units are to be regarded as standard. No other units of measurement are included in this standard. 1.4 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. |
||||
2. Referenced Documents | ||||
|
Historická
1.3.2013
Historická
1.10.2011
Historická
1.10.2014
Historická
15.4.2011
Historická
1.5.2008
Historická
1.10.2014
Posledná aktualizácia: 2024-11-21 (Počet položiek: 2 206 478)
© Copyright 2024 NORMSERVIS s.r.o.