Standard Test Methods for Oxidation Onset Temperature of Hydrocarbons by Differential Scanning Calorimetry (Includes all amendments And changes 2/2/2023).
Automaticky preložený názov:
Štandardné skúšobné metódy pre oxidačné teplotou nástupu uhľovodíkov diferenčný skenovací kalorimetria
NORMA vydaná dňa 15.3.2014
Označenie normy: ASTM E2009-08(2014)e1
Poznámka: NEPLATNÁ
Dátum vydania normy: 15.3.2014
Kód tovaru: NS-43939
Počet strán: 5
Približná hmotnosť: 15 g (0.03 libier)
Krajina: Americká technická norma
Kategória: Technické normy ASTM
Keywords:
differential scanning calorimetry, differential thermal analysis, hydrocarbons, oxidation, oxidation induction time (OIT), oxidation onset temperature (OOT), oxidative stability, pressure differential scanning calorimetry, ICS Number Code 17.200.10 (Heat. Calorimetry)
Significance and Use | ||||||||||||||||
5.1 Oxidation onset temperature is a relative measure of the degree of oxidative stability of the material evaluated at a given heating rate and oxidative environment, for example, oxygen; the higher the OOT value the more stable the material. The OOT is described in Fig. 1. The OOT values can be used for comparative purposes and are not an absolute measurement, like the oxidation induction time (OIT) at a constant temperature (see Test Method E1858). The presence or effectiveness of antioxidants may be determined by these test methods. 5.2 Typical uses of these test methods include the oxidative stability of edible oils and fats (oxidative rancidity), lubricants, greases, and polyolefins. |
||||||||||||||||
1. Scope | ||||||||||||||||
1.1 These test methods describe the determination of the oxidative properties of hydrocarbons by differential scanning calorimetry or pressure differential scanning calorimetry under linear heating rate conditions and are applicable to hydrocarbons, which oxidize exothermically in their analyzed form. 1.2 Test Method A—A differential scanning calorimeter (DSC) is used at ambient pressure, of one atmosphere of oxygen. 1.3 Test Method B—A pressure DSC (PDSC) is used at high pressure, for example, 3.5 MPa (500 psig) oxygen. 1.4 Test Method C—A differential scanning calorimeter (DSC) is used at ambient pressure of one atmosphere of air. 1.5 The values stated in SI units are to be regarded as standard. No other units of measurement are included in this standard. 1.6 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. |
||||||||||||||||
2. Referenced Documents | ||||||||||||||||
|
Chcete mať istotu, že používate len platné technické normy?
Ponúkame Vám riešenie, ktoré Vám zaistí mesačný prehľad o aktuálnosti noriem, ktoré používate.
Chcete vedieť viac informácií ? Pozrite sa na túto stránku.
Posledná aktualizácia: 2024-11-13 (Počet položiek: 2 210 764)
© Copyright 2024 NORMSERVIS s.r.o.