Standard Test Method for Multiple Stress Creep and Recovery (MSCR) of Asphalt Binder Using a Dynamic Shear Rheometer (Includes all amendments And changes 1/11/2016).
Automaticky preložený názov:
Štandardná skúšobná metóda pre Multiple stresu Creep and Recovery (rkp) zo asfaltového spojiva pomocou dynamického nožnice Rheometer
NORMA vydaná dňa 1.6.2010
Označenie normy: ASTM D7405-10a
Poznámka: NEPLATNÁ
Dátum vydania normy: 1.6.2010
Kód tovaru: NS-38380
Počet strán: 4
Približná hmotnosť: 12 g (0.03 libier)
Krajina: Americká technická norma
Kategória: Technické normy ASTM
Keywords:
asphalt binder, creep and recovery, DSR, dynamic shear rheometer, elastic recovery, MSCR, non-recoverable creep compliance, polymer modified asphalt, Asphalt binder, MSCR (multiple stress creep and recovery), Multiple stress creep and recovery (MSCR), Rheometers, ICS Number Code 91.100.50 (Binders. Sealing materials)
Significance and Use | ||||||||||||||||
This test method is used to identify the presence of elastic response in a binder and the change in elastic response at two different stress levels. Non-recoverable creep compliance has been shown to be an indicator of the resistance of an asphalt binder to permanent deformation under repeated load. This test method is also useful as a surrogate for other test methods used to measure elasticity in asphalt binders such as Test Method D5801 (Toughness and Tenacity), Test Method D6084 (Elastic Recovery), and Test Method D7175 (DSR phase angle). |
||||||||||||||||
1. Scope | ||||||||||||||||
1.1 This test method covers the determination of percent recovery and non-recoverable creep compliance of asphalt binders by means of Multiple Stress Creep and Recovery (MSCR) testing. The MSCR test is conducted using the Dynamic Shear Rheometer (DSR) at a specified temperature. 1.2 This standard is appropriate for unaged material, material aged in accordance with Test Method D2872 (RTFO), material aged in accordance with Practice D6521 (PAV), and material aged in accordance with both Test Method D2872 and Practice D6521. Note 1—The majority of development work on this test method was performed on material aged in accordance with Test Method D2872 (RTFO). 1.3 The percent recovery is intended to provide a means to determine the presence of elastic response and stress dependence of polymer modified and unmodified asphalt binders. 1.4 The values stated in SI units are to be regarded as standard. No other units of measurement are included in this standard. 1.5 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. |
||||||||||||||||
2. Referenced Documents | ||||||||||||||||
|
Chcete mať istotu, že používate len platné technické normy?
Ponúkame Vám riešenie, ktoré Vám zaistí mesačný prehľad o aktuálnosti noriem, ktoré používate.
Chcete vedieť viac informácií ? Pozrite sa na túto stránku.
Posledná aktualizácia: 2024-12-23 (Počet položiek: 2 217 157)
© Copyright 2024 NORMSERVIS s.r.o.