Standard Practice for Evaluating Coatings Applied Over Surfaces Treated With Inhibitors Used to Prevent Flash Rusting of Steel When Water or Water/Abrasive Blasted
Automaticky preložený názov:
Štandardná prax pre hodnotenie povlaky nanášané sa povrchy liečených inhibítormi používa na zabránenie šíreniu korózie oceľových Keď voda alebo voda / abrazívne Blasted
NORMA vydaná dňa 1.1.2008
Označenie normy: ASTM D5367-08
Poznámka: NEPLATNÁ
Dátum vydania normy: 1.1.2008
Kód tovaru: NS-30903
Počet strán: 3
Približná hmotnosť: 9 g (0.02 libier)
Krajina: Americká technická norma
Kategória: Technické normy ASTM
Keywords:
abrasive blasting, coatings, inhibitors, surface preparation, water blasting, Substrates--coating applications, Surface preparation--paints/related coatings, Abrasive blasting, Coatings (paint/related applications), Inhibitors, Water treatment applications, ICS Number Code 87.040 (Paints and varnishes)
Significance and Use | ||||||||||||||||||||
Water-blast cleaning with, (SSPC-TR2/NACE 6C 198) or without, (SSPC-SP 12/NACE No. 5) abrasive, results in flash rusting under some environmental conditions. Inhibitors are used to prevent flash rusting while drying and before coating application. The inhibitor or reaction products of the inhibitor on the substrate becomes part of the coating systems. Coating performance may be influenced by the inhibitor. Soluble contaminants or unreacted inhibitors left on the surface under the coating may cause premature failure. This practice includes a comparison of coating performance with and without inhibitors using various laboratory tests to simulate a range of conditions such as high moisture, marine atmospheric or water immersion. The user or specifier must determine the specific test methods to be used and exposure conditions. Some test methods referenced may not be applicable to all types of coatings. |
||||||||||||||||||||
1. Scope | ||||||||||||||||||||
1.1 This practice covers procedures to evaluate the compatibility of coatings with inhibitors used to prevent flash rusting of steel before application of coatings. 1.2 The inhibitors are used with water-blast cleaning surface preparation and may be used with or without abrasives. 1.3 The manufacturer of the coatings shall be consulted to ensure compatibility of inhibitors with the coatings. 1.4 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. |
||||||||||||||||||||
2. Referenced Documents | ||||||||||||||||||||
|
Chcete mať istotu, že používate len platné technické normy?
Ponúkame Vám riešenie, ktoré Vám zaistí mesačný prehľad o aktuálnosti noriem, ktoré používate.
Chcete vedieť viac informácií ? Pozrite sa na túto stránku.
Posledná aktualizácia: 2024-12-22 (Počet položiek: 2 217 000)
© Copyright 2024 NORMSERVIS s.r.o.