Standard Test Methods for Chemical and Gravimetric Analysis of White and Yellow Thermoplastic Traffic Marking Containing Lead Chromate and Titanium Dioxide
Automaticky preložený názov:
Štandardné testovacie metódy pre chemické a Gravimetrická analýza bielej a žltej termoplastického dopravné značenie , ktoré obsahujú olovo Chromate a oxid titaničitý
NORMA vydaná dňa 10.10.1998
Označenie normy: ASTM D4797-88(1998)
Poznámka: NEPLATNÁ
Dátum vydania normy: 10.10.1998
Kód tovaru: NS-28604
Počet strán: 3
Približná hmotnosť: 9 g (0.02 libier)
Krajina: Americká technická norma
Kategória: Technické normy ASTM
Keywords:
Chemical analysis-paints/related coatings/materials, Furnaces, Glass spheres (in traffic paint/marking material), Gravimetric method, Heating tests-paints/related coatings/materials, Lead chromate pigment, Muffle-furnace technique, Pigments-lead chromate, Pigments-titanium dioxide, Residue, Temperature (application), Thermoplastic traffic marking material, Titanium dioxide (TiO[inf]2[reset]), white/yellow thermoplastic traffic marking material (containing lead
| 1. Scope | ||||||||||||
|
1.1 These test methods cover procedures for the chemical and gravimetric analysis of white and yellow thermoplastic traffic marking containing lead chromate and titanium dioxide pigment. 1.2 The analytical procedures appear in the following order: Sections Percent Binder 10 Percent Glass Beads (Note 1) 11 Percent Titanium Dioxide 12 Percent Lead Chromate and Analysis of Chrome Yellow and 13 Chrome Orange Pigments (Note 2)1.3 This standard does not purport to address all of the safety problems, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. Note 1-Test for 1.50 glass spheres only. Note 2-This modified analysis of chrome yellow and chrome orange pigments must be used because the heat resistant chrome yellows in the thermoplastic cannot be analyzed by Test Method D126. |
||||||||||||
| 2. Referenced Documents | ||||||||||||
|
Chcete mať istotu, že používate len platné technické normy?
Ponúkame Vám riešenie, ktoré Vám zaistí mesačný prehľad o aktuálnosti noriem, ktoré používate.
Chcete vedieť viac informácií ? Pozrite sa na túto stránku.
Posledná aktualizácia: 2026-09-08 (Počet položiek: 2 300 134)
© Copyright 2026 NORMSERVIS s.r.o.