Standard Test Methods for Rubber-Determination of Ethylene Units in Ethylene-Propylene Copolymers (EPM) and in Ethylene-Propylene-Diene Terpolymers (EPDM) by Infrared Spectrometry (Includes all amendments And changes 7/29/2015).
Automaticky preložený názov:
Štandardné skúšobné metódy pre gumový stanovenie etylénu jednotiek v kopolyméry etylénu a propylénu (EPM) a etylén-propylén-dién (EPDM) pomocou infračervenej spektrometrie
NORMA vydaná dňa 1.6.2010
Označenie normy: ASTM D3900-05a(2010)
Poznámka: NEPLATNÁ
Dátum vydania normy: 1.6.2010
Kód tovaru: NS-25281
Počet strán: 9
Približná hmotnosť: 27 g (0.06 libier)
Krajina: Americká technická norma
Kategória: Technické normy ASTM
Keywords:
ethylene-propylene copolymers, ethylene-propylene-diene terpolymers, infrared, Cast film method, Chemical analysis--rubber chemicals/materials, EPM/EPDM materials/applications, Ethylene-propylene copolymers, Infrared (IR) analysis--rubber, Infrared spectrophotometry, Pressed film method, Raw rubber, ICS Number Code 83.040.10 (Latex and raw rubber)
Significance and Use | ||||||||
These test methods can be used for determining which EPDM polymers are evaluated in the different compounds in Test Methods D3568. Differences in ethylene sequence distribution cause differences in crystallinity and green strength at the same ethylene content. Since these are important variables in EPM and EPDM processability and end-use properties, the ethylene content of the rubber should not be used as the sole measurement to determine the suitability of a particular rubber for an intended purpose. |
||||||||
1. Scope | ||||||||
1.1 These test methods cover the determination of the proportion of ethylene and propylene units in ethylene-propylene copolymers (EPM) and ethylene-propylenediene terpolymers (EPDM) over the range from 35 to 85 mass % ethylene. Four test methods are needed to encompass the variety of commercial polymers that contain additives or polymerized diene units that interfere with the various infrared peaks. Except when interferences are present, all four test methods should give similar results. The test methods appear in the following order: |
||||||||
2. Referenced Documents | ||||||||
|
Poskytovanie aktuálnych informácií o legislatívnych predpisoch vyhlásených v Zbierke zákonov od roku 1945.
Aktualizácia 2x v mesiaci !
Chcete vedieť viac informácii ? Pozrite sa na túto stránku.
Posledná aktualizácia: 2024-11-22 (Počet položiek: 2 206 568)
© Copyright 2024 NORMSERVIS s.r.o.