Standard Test Method for 2,6-di-tert-Butyl- p-Cresol and 2,6-di-tert-Butyl Phenol in Electrical Insulating Oil by Infrared Absorption
Automaticky preložený názov:
Štandardná skúšobná metóda pre 2,6-di-terc-butyl-p-kresol a 2,6-di-terc-butyl-fenolu v elektroizolačné olej Infračervené absorpčné
NORMA vydaná dňa 1.11.2013
Označenie normy: ASTM D2668-07(2013)
Poznámka: NEPLATNÁ
Dátum vydania normy: 1.11.2013
Kód tovaru: NS-21098
Počet strán: 6
Približná hmotnosť: 18 g (0.04 libier)
Krajina: Americká technická norma
Kategória: Technické normy ASTM
Keywords:
2,6-ditertiary-butyl paracresol, 2,6-ditertiary-butyl phenol, electrical insulating oil, infrared absorption, ICS Number Code 29.040.10 (Insulating oils)
Significance and Use | ||||||
3.1 The quantitative determination of 2,6-ditertiary-butyl paracresol and 2,6-ditertiary-butyl phenol in a new electrical insulating oil measures the amount of this material that has been added to the oil as protection against oxidation. In a used oil it measures the amount remaining after oxidation has reduced its concentration. The test is also suitable for manufacturing control and specification acceptance. 3.2 When an infrared spectrum is obtained of an electrical insulating oil inhibited with either of these compounds there is an increase in absorbance of the spectrum at several wavelengths (or wavenumbers). 2,6 ditertiary-butyl paracresol produces pronounced increases in absorbance at 2.72 μm (3650 cm−1), and 11.63 μm (860 cm−1 ). 2,6 ditertiary-butyl phenol produces pronounced increases in absorbance at 2.72 μm (3650 cm−1) and 13.42 μm (745 cm −1). 3.3 When making this test on other than a highly oxidized oil or when using a double-beam spectrophotometer, it has been found convenient to obtain the spectrum between 2.5 μm (4000 cm−1) and 2.9 μm (3450 cm−1) because the instrument is compensated for the presence of moisture and the band is not influenced by intermolecular forces (associations). However, when testing a highly oxidized oil or when using a single-beam instrument better results may be obtained if the scan is made between 10.90 μm (918 cm−1) and 14.00 μm (714 cm−1). 3.4 Increased absorption at 11.63 μm (860 cm −1) or 13.42 μm (745 cm−1) or both, will identify the inhibitor as 2,6-ditertiary-butyl paracresol or 2,6-ditertiary-butyl phenol respectively (Note 1). 1.1 This test method covers the
determination of the weight percent of 2,6-ditertiary-butyl
paracresol (DBPC) and 2,6-ditertiary-butyl phenol (DBP) in new or
used electrical insulating oil in concentrations up to 0.5 % by
measuring its absorbance at the specified wavelengths in the
infrared spectrum.
1.2 The values stated in SI units are to be regarded as standard. No other units of measurement are included in this standard. 1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. |
||||||
2. Referenced Documents | ||||||
|
Historická
1.12.2009
Historická
15.5.2009
Historická
1.5.2013
Historická
1.11.2006
Historická
15.5.2010
Historická
1.8.2011
Posledná aktualizácia: 2025-01-21 (Počet položiek: 2 220 867)
© Copyright 2025 NORMSERVIS s.r.o.