Potrebujeme váš súhlas na využitie jednotlivých dát, aby sa vám okrem iného mohli ukazovať informácie týkajúce sa vašich záujmov. Súhlas udelíte kliknutím na tlačidlo „OK“.
Standard Test Method for Drying Shrinkage of Mortar Containing Hydraulic Cement
Automaticky preložený názov:
Štandardná skúšobná metóda pre zmrštenie sušením malty obsahujúce hydraulického cementu
NORMA vydaná dňa 1.6.2007
Označenie normy: ASTM C596-07
Poznámka: NEPLATNÁ
Dátum vydania normy: 1.6.2007
Kód tovaru: NS-14188
Počet strán: 3
Približná hmotnosť: 9 g (0.02 libier)
Krajina: Americká technická norma
Kategória: Technické normy ASTM
Keywords:
drying shrinkage, hydraulic cement, method, mortar, ICS Number Code 91.100.10 (Cement. Gypsum. Lime. Mortar)
| Significance and Use | ||||||||||||||||||
|
This test method establishes a selected set of conditions of temperature, relative humidity and rate of evaporation of the environment to which a mortar specimen of stated composition shall be subjected for a specified period of time during which its change in length is determined and designated “drying shrinkage”. The drying shrinkage of mortar as determined by this test method has a linear relation to the drying shrinkage of concrete made with the same cement and exposed to the same drying conditions.4 Hence this test method may be used when it is desired to develop data on the effect of a hydraulic cement on the drying shrinkage of concrete made with that cement. |
||||||||||||||||||
| 1. Scope | ||||||||||||||||||
|
1.1 This test method determines the change in length on drying of mortar bars containing hydraulic cement and graded standard sand. 1.2 The values stated in SI units are to be regarded as the standard. Values given in parentheses are for information only. This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. (Warning- Fresh hydraulic cementitious mixtures are caustic and may cause chemical burns to skin and tissue upon prolonged exposure). |
||||||||||||||||||