Standard Specification for Hydrated Lime for Masonry Purposes
NORMA vydaná dňa 1.10.2018
Označenie normy: ASTM C207-18
Poznámka: NEPLATNÁ
Dátum vydania normy: 1.10.2018
Kód tovaru: NS-904606
Počet strán: 2
Približná hmotnosť: 6 g (0.01 libier)
Krajina: Americká technická norma
Kategória: Technické normy ASTM
Keywords:
hydrated lime, masonry, mortar, plasticity, popping and pitting, residue, stucco, Type N, Type NA, Type S, Type SA, unhydrated oxides, water retention, air entraining ,, ICS Number Code 91.100.10 (Cement. Gypsum. Lime. Mortar)
1. Scope | ||||||||||||||
1.1 This specification covers four types of hydrated lime. Types N and S are suitable for use in mortar, in scratch and brown coats of cement plaster, for stucco, and for addition to portland-cement concrete. Types NA and SA are air-entrained hydrated limes that are suitable for use in any of the above uses where the inherent properties of lime and air-entrainment are desired. The four types of lime sold under this specification shall be designated as follows: 1.1.1 Type N—Normal hydrated lime for masonry purposes. 1.1.2 Type S—Special hydrated lime for masonry purposes. 1.1.3 Type NA—Normal air-entraining hydrated lime for masonry purposes. 1.1.4 Type SA—Special air-entraining hydrated lime for masonry purposes. Note 1: Type S, special hydrated lime, and Type SA, special
air-entraining hydrated lime, are differentiated from Type N,
normal hydrated lime, and Type NA, normal air-entraining hydrated
lime, principally by their ability to develop high, early
plasticity and higher water retentivity, and by a limitation on
their unhydrated oxide content.
Note 2: For normal (Type N) and special (Type S) finishing
hydrated lime, refer to Specification C206.
Note 3: Some building codes prohibit the use of air-entraining
materials in mortar, because of the accompanying reduction in bond
and compressive strength. Where increased freeze-thaw resistance is
important, air-entraining may be beneficial. Air-entraining lime
should not be used as a finishing lime.
Note 4: For lime putty, refer to Specification C1489.
1.2 The values stated in SI units are to be regarded as standard. 1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety, health, and environmental practices and determine the applicability of regulatory limitations prior to use. 1.4 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee. |
||||||||||||||
2. Referenced Documents | ||||||||||||||
|
Chcete mať istotu o platnosti využívaných predpisov?
Ponúkame Vám riešenie, aby ste mohli používať stále platné (aktuálne) legislatívne predpisy
Chcete vedieť viac informácií ? Pozrite sa na túto stránku.
Posledná aktualizácia: 2024-11-21 (Počet položiek: 2 206 478)
© Copyright 2024 NORMSERVIS s.r.o.