Potrebujeme váš súhlas na využitie jednotlivých dát, aby sa vám okrem iného mohli ukazovať informácie týkajúce sa vašich záujmov. Súhlas udelíte kliknutím na tlačidlo „OK“.
Standard Specification for Hydrated Lime for Masonry Purposes
Automaticky preložený názov:
Štandardné špecifikácie pre vápenného hydrátu pre murivo účely
NORMA vydaná dňa 1.2.2004
Označenie normy: ASTM C207-04
Poznámka: NEPLATNÁ
Dátum vydania normy: 1.2.2004
Kód tovaru: NS-12531
Počet strán: 2
Približná hmotnosť: 6 g (0.01 libier)
Krajina: Americká technická norma
Kategória: Technické normy ASTM
Keywords:
hydrated lime, masonry, plasticity, popping and pitting, residue, stucco, Type N, Type NA, Type S, Type SA, unhydrated oxides, water retention, air entraining, ICS Number Code 91.100.10 (Cement. Gypsum. Lime. Mortar)
| 1. Scope | ||||||||||||||
|
1.1 This specification covers four types of hydrated lime. Types N and S are suitable for use in mortar, in scratch and brown coats of cement plaster, for stucco, and for addition to portland-cement concrete. Types NA and SA are air-entrained hydrated limes that are suitable for use in any of the above uses where the inherent properties of lime and air-entrainment are desired. The four types of lime sold under this specification shall be designated as follows: 1.1.1 Type N—Normal hydrated lime for masonry purposes. 1.1.2 Type S—Special hydrated lime for masonry purposes. 1.1.3 Type NA— Normal air-entraining hydrated lime for masonry purposes. 1.1.4 Type SA—Special air-entraining hydrated lime for masonry purposes. Note 1—Type S, special hydrated lime, and Type SA, special air-entraining hydrated lime, are differentiated from Type N, normal hydrated lime, and Type NA, normal air-entraining hydrated lime, principally by their ability to develop high, early plasticity and higher water retentivity, and by a limitation on their unhydrated oxide content. Note 2—For normal (Type N) and special (Type S) finishing hydrated lime, refer to Specification C 206. Note 3Some building codes prohibit the use of air-entraining materials in mortar, because of the accompanying reduction in bond and compressive strength. Where increased freeze-thaw resistance is important, air-entraining may be beneficial. Air-entraining lime should not be used as a finishing lime. Note 4—For lime putty, refer to Specification C 1489. 1.2 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. |
||||||||||||||
| 2. Referenced Documents | ||||||||||||||
|
Chcete mať istotu, že používate len platné technické normy?
Ponúkame Vám riešenie, ktoré Vám zaistí mesačný prehľad o aktuálnosti noriem, ktoré používate.
Chcete vedieť viac informácií ? Pozrite sa na túto stránku.
Posledná aktualizácia: 2026-06-21 (Počet položiek: 2 283 476)
© Copyright 2026 NORMSERVIS s.r.o.