Potrebujeme váš súhlas na využitie jednotlivých dát, aby sa vám okrem iného mohli ukazovať informácie týkajúce sa vašich záujmov. Súhlas udelíte kliknutím na tlačidlo „OK“.
Standard Specification for Finishing Hydrated Lime
Automaticky preložený názov:
Štandardné špecifikácie pre dokončovacie vápenného hydrátu
NORMA vydaná dňa 1.12.2009
Označenie normy: ASTM C206-03(2009)
Poznámka: NEPLATNÁ
Dátum vydania normy: 1.12.2009
Kód tovaru: NS-12527
Počet strán: 2
Približná hmotnosť: 6 g (0.01 libier)
Krajina: Americká technická norma
Kategória: Technické normy ASTM
Keywords:
finishing lime, masonry, plaster, plasticity, popping and pitting, residue, Type N, Type S, unhydrated oxides, Cement materials/applications--specifications, Finishing process/finishes, Hydrated lime--specifications, ICS Number Code 91.100.10 (Cement. Gypsum. Lime. Mortar)
1. Scope | ||||||||||||||||
1.1 This specification covers two types of finishing hydrated lime that are suitable for use in the scratch, brown, and finish coats of plaster, for stucco, for mortar, and as an addition to portland-cement concrete. The two types of lime sold under this specification shall be designated as follows: 1.1.1 Type N—Normal hydrated lime for finishing purposes, and 1.1.2 Type S—Special hydrated lime for finishing purposes. Note 1—Type N, normal finishing hydrated lime, is differentiated from Type S, special finishing hydrated lime, in that no limitation on the amount of unhydrated oxides is specified for Type N hydrate, and the plasticity requirement for Type N hydrate shall be determined after soaking for 16 to 24 h. Note 2—For lime putty, refer to Specification C1489. 1.2 The values stated in inch-pound units are to be regarded as standard. The values given in parentheses are mathematical conversions to SI units that are provided for information only and are not considered standard. |
||||||||||||||||
2. Referenced Documents | ||||||||||||||||
|
Posledná aktualizácia: 2024-11-03 (Počet položiek: 2 209 203)