Standard Test Method for Interlaminar Shear Strength of 1-D and 2-D Continuous Fiber-Reinforced Advanced Ceramics at Elevated Temperatures
Automaticky preložený názov:
Štandardná skúšobná metóda pre interlaminálna pevnosti v šmyku 1 - D a 2 - D Kontinuálne vystužené vláknami Pokročilé Keramika pri zvýšených teplotách
NORMA vydaná dňa 1.2.2005
Označenie normy: ASTM C1425-05
Poznámka: NEPLATNÁ
Dátum vydania normy: 1.2.2005
Kód tovaru: NS-11196
Počet strán: 8
Približná hmotnosť: 24 g (0.05 libier)
Krajina: Americká technická norma
Kategória: Technické normy ASTM
Keywords:
composite, compression, continuous fiber-reinforced ceramic composite (CFCC), interlaminar, shear, shear strength, ICS Number Code 81.060.30 (Advanced ceramics)
Significance and Use | ||||||||||||||||||||||||||
Continuous fiber-reinforced ceramic composites are candidate materials for structural applications requiring high degrees of wear and corrosion resistance, and damage tolerance at high temperatures. The 1-D and 2-D CFCCs are highly anisotropic and their transthickness tensile and interlaminar shear strength are lower than their in-plane tensile and in-plane shear strength, respectively. Shear tests provide information on the strength and deformation of materials under shear stresses. This test method may be used for material development, material comparison, quality assurance, characterization, and design data generation. For quality control purposes, results derived from standardized shear test specimens may be considered indicative of the response of the material from which they were taken for given primary processing conditions and post-processing heat treatments. |
||||||||||||||||||||||||||
1. Scope | ||||||||||||||||||||||||||
1.1 This test method addresses the compression of a double-notched specimen to determine interlaminar shear strength of continuous fiber-reinforced ceramic composites (CFCCs) at elevated temperatures. Specimen preparation methods and requirements, testing modes (load or displacement control), testing rates (load rate or displacement rate), data collection, and reporting procedures are addressed. 1.2 This test method is used for testing advanced ceramic or glass matrix composites with continuous fiber reinforcement having a laminated structure such as in unidirectional (1-D) or bidirectional (2-D) fiber architecture (lay-ups of unidirectional plies or stacked fabric). This test method does not address composites with nonlaminated structures, such as (3-D) fiber architecture or discontinuous fiber-reinforced, whisker-reinforced, or particulate-reinforced ceramics. 1.3 Values expressed in this test method are in accordance with the International System of Units (SI) and IEEE/ASTM SI 10. This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. Specific precautionary statements are noted in and . |
||||||||||||||||||||||||||