Potrebujeme váš súhlas na využitie jednotlivých dát, aby sa vám okrem iného mohli ukazovať informácie týkajúce sa vašich záujmov. Súhlas udelíte kliknutím na tlačidlo „OK“.
Standard Specification for Flat-Rolled, Grain-Oriented, Silicon-Iron, Electrical Steel, Fully Processed Types
Automaticky preložený názov:
Štandardné špecifikácie pre ploché valcované , s orientovanou štruktúrou , Silicon - Iron , elektrické oceľ, Plne spracované druhy
NORMA vydaná dňa 1.5.2009
Označenie normy: ASTM A876-09
Poznámka: NEPLATNÁ
Dátum vydania normy: 1.5.2009
Kód tovaru: NS-4604
Počet strán: 6
Približná hmotnosť: 18 g (0.04 libier)
Krajina: Americká technická norma
Kategória: Technické normy ASTM
Keywords:
electrical steel, grain-oriented, high permeability, A-C (alternating-current) magnetic properties, Alloy steel bars--specifications, Alternating-current permeability, Electrical contact materials--specifications, Electrical steel (oriented)--specifications, Flat-rolled electrical steel, Grain oriented electrical steel, Induction, Magnetic materials/applications--specifications, Metallurgical structure, Oriented electrical steel--specifications, Silicon electrical steel, Transformer cores
| 1. Scope | ||||||||||||||||||||||||
|
1.1 This specification covers the detailed requirements to which the specified grades of flat-rolled, grain-oriented, fully processed electrical steels shall conform. These steels are used primarily in transformer cores operating at moderate to high magnetic flux densities at commercial power frequencies (50 and 60 Hz). 1.2 These grain-oriented electrical steels are low-carbon, silicon-iron alloys with a silicon content of approximately 3.2 % in which low core loss and high permeability in the direction of rolling have been achieved by appropriate metallurgical processing. 1.3 The electrical-steel grades described in this specification include (1) conventional grain-oriented electrical steel tested at 15 kG (1.5 T) in accordance with Test Method A 343/A 343M, (2) conventional grain-oriented electrical steel tested at 17 kG (1.7 T) in accordance with Test Method A 343/A 343M, (3) high-permeability grain-oriented electrical steel tested at 17 kG (1.7 T) in accordance with Test Method A 343/A 343M, and (4) laser-scribed high-permeability grain-oriented electrical steel tested at 17 kG (1.7 T) in accordance with Test Methods A 804/A 804M. 1.4 The values stated in customary (cgs-emu and inch-pound) units are to be regarded as standard. The values given in parentheses are mathematical conversions to SI units, which are provided for information only and are not considered standard. |
||||||||||||||||||||||||
| 2. Referenced Documents | ||||||||||||||||||||||||
|