Standard Test Method for dc Magnetic Properties of Materials Using Ring and Permeameter Procedures with dc Electronic Hysteresigraphs
Automaticky preložený názov:
Štandardná skúšobná metóda pre jednosmerné magnetické vlastnosti materiálov s využitím Ring a permeametr postupy s dc Electronic Hysteresigraphs
NORMA vydaná dňa 10.6.2001
Označenie normy: ASTM A773/A773M-01
Poznámka: NEPLATNÁ
Dátum vydania normy: 10.6.2001
Kód tovaru: NS-4113
Počet strán: 10
Približná hmotnosť: 30 g (0.07 libier)
Krajina: Americká technická norma
Kategória: Technické normy ASTM
Keywords:
dc hysteresigraph, dc hysteresis, Epstein test, Hall probe, hysteresis loop, permeameter, ring-type specimen, ICS Number Code 29.030 (Magnetic materials)
| Significance and Use | ||||||||||||||||
|
Hysteresigraph testing permits more rapid and efficient collection of dc hysteresis (B-H loop) data as compared to the point by point ballistic Test Methods A 341/A 341M and A 596/A 596M. The accuracy and precision of testing is comparable to the ballistic methods. Hysteresigraphs are particularly desirable for testing of semihard and hard magnetic materials where either the entire second quadrant (demagnetization curve) or entire hysteresis loop is of primary concern. Provided the test specimen is representative of the bulk sample or lot, this test method is well suited for design, specification acceptance, service evaluation and research and development. |
||||||||||||||||
| 1. Scope | ||||||||||||||||
|
1.1 This test method provides dc hysteresigraph procedures ( B-H loop methods) for the determination of basic magnetic properties of materials in the form of ring, toroidal, link, double-lapped Epstein cores, or other standard shapes that may be cut, stamped, machined, or ground from cast, compacted, sintered, forged, or rolled materials. It includes tests for normal induction and hysteresis taken under conditions of continuous sweep magnetization. Rate of sweep may be varied, either manually or automatically at different portions of the curves during tracing. Total elapsed time for tracing a hysteresis loop is commonly 10 to 120 s per loop. 1.2 The values stated in either customary (cgs-emu and inch-pound) units or SI units are to be regarded separately as standard. Within the text, the SI units are shown in brackets. The values stated in each system are not exact equivalents; therefore, each system shall be used independently of the other. Combining values from the systems may result in nonconformance with this test method. 1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. |
||||||||||||||||
| 2. Referenced Documents | ||||||||||||||||
|
Chcete mať istotu, že používate len platné technické normy?
Ponúkame Vám riešenie, ktoré Vám zaistí mesačný prehľad o aktuálnosti noriem, ktoré používate.
Chcete vedieť viac informácií ? Pozrite sa na túto stránku.
Posledná aktualizácia: 2026-04-28 (Počet položiek: 2 274 955)
© Copyright 2026 NORMSERVIS s.r.o.