Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 41.5Ni - 16Cr - 37Fe - 2.9Cb (Nb) - 1.8Ti Consumable Electrode Remelted or Vacuum Induction Melted 1800 °F (982 °C) Solution Heat Treated
NORMA vydaná dňa 1.7.2015
Designation standards: SAE AMS5701E
Note: Neaktuálna
Publication date standards: 1.7.2015
Country: American technical standard
Kategória: Technické normy SAE