Standard Specification for High-Strength Steel Castings in Heavy Sections
NORMA vydaná dňa 1.9.2018
Prečo Redline?
Redline predstavuje rýchly a jednoduchý spôsob ako porovnať všetky zmeny medzi aktuálne platnou normou a predchádzajúcou verziou.
Vďaka redline sa okamžite dozviete o:
Ušetrite si čas aj starosti!
Vďaka Redline už nebudete musieť strácať čas zisťovaním, čo sa v novej norme zmenilo. Redline Vám ušetrí čas a zaručí, že sa o zmenách v norme dozviete.
Cena
Ak si zvolíte možnosť "Platná norma + Redline", potom dostanete oba dokumenty! A čo je najlepšie, cena Platné normy + Redline je len o niečo málo vyššia ako cena samostatnej platné normy.
Designation standards: ASTM A1001-18
Publication date standards: 1.9.2018
The number of pages: 6
Approximate weight : 18 g (0.04 lbs)
Country: American technical standard
Kategória: Technické normy ASTM
This specification covers cast alloy steels in the normalized and tempered or quenched and tempered condition, suitable for high strain gradient conditions. One test block for each heat is required. The test block configuration and size are specified. Tension and Charpy impact tests and oxygen, nitrogen, and hydrogen gas content tests shall be performed. The steel shall be made by electric furnace process with methods, such as argon-oxygen-decarburization, to conform to the maximum gas level. Heat treatment procedure shall be done. Multiple austenitizing and tempering are permitted. The chemistry grade shall conform to the required chemical composition for carbon, manganese, phosphorus, sulfur, silicon, nickel, chromium, molybdenum, and aluminum. Residual elements include: zirconium, copper, titanium, tungsten, vanadium, columbium, and boron. A product analysis shall be made for specification conformance. Casting shell and core depth zone shall be established and examined. Repair methods such as grinding and welding are detailed.
Keywords:
aluminum nitride, AOD, heavy section, hydrogen gas, nitrogen gas, oxygen gas,, ICS Number Code 77.140.80 (Iron and steel castings)